AI concept illustration of a cup, sealing film and holder shown separately
AI-generated concept illustration. No WJPETCUP model, assembled sealing combination or leakage test is represented.

Preserve the fault before changing the setup

If this cup, film and machine combination has not been confirmed for film sealing, start with the heat-sealing compatibility guide before investigating a production fault.

Do not serve or distribute packs with a failed seal and identify the associated cup carton, film roll and time of production. Retain an unused sample from each relevant component where practical. Photograph the failure before peeling off the film: peeling changes the evidence at the interface. Record which observations were made before and after opening.

Observe only from the machine’s normal safe operating position. For cleaning or inspection that requires access, stop and follow the exact model’s shutdown, power-isolation and cooling instructions. BubbleTeaology explicitly requires power disconnection before maintenance. Do not remove guards, defeat interlocks or carry out electrical checks to follow this article. An equipment fault or unsafe movement belongs with the equipment supplier or an authorized technician.

Choose the branch from the stage of the failure

“The cup leaks” is an outcome, not a diagnosis. Identify the earliest abnormal event you can observe safely. BubbleTeaology’s equipment guide treats film breakage, failure to stop in position and a cup receiving only a small piece of film as different problems. That distinction is useful even when your machine has different controls: a film-feed problem should not be recorded simply as a weak bond.

Use the table to decide what evidence to collect. Its entries are investigation routes, not a list of confirmed causes or instructions to adjust equipment.

Route the observation before choosing a remedy
First observed problemUseful recordNext investigation
Film sticks or tears before reaching the cup.Roll identity, point of breakage, remaining roll size and when the problem began.Film supplier and equipment supplier review the roll and its approved feed arrangement; no seal-temperature conclusion follows yet.
Print or cut position drifts, or only part of the cup receives film.The observed cycle, recorded from the normal safe operating position; registration-mark and cut positions; the installed roll specification.Equipment supplier checks positioning against the exact model’s instructions; film supplier confirms the printed repeat and roll format.
One arc of the rim is weak or a crease crosses the sealing area.Top and side photographs, defect location and whether it repeats in the same orientation.Review rim condition, filling residue, cup support and film presentation before assuming a material mismatch.
Film covers the rim but separates unusually easily.Where separation occurs, the intended opening behaviour and the agreed test result.Check the specified sealing layer and operating conditions; a hand peel alone cannot distinguish an intended easy-peel design from an unacceptable seal.
The pack appears acceptable initially but fails after holding or handling.Time, contents, fill level, storage and handling between sealing and failure.Assess the finished pack under those actual conditions; the immediate observation does not establish later performance.

Record where the defect appears, not just how it looks

For a local gap, describe the location relative to both the cup and the machine. A photo of “the left side” becomes ambiguous after someone rotates the cup. Keep a consistent viewing direction and include an identifiable feature in the photograph where one exists. Do not mark or contaminate the sealing surface to create a reference.

Edelstein’s alignment guidance distinguishes a recurring weak area from a defect that changes position. Repeated location can justify checking contact and support; changing location can justify reviewing component variation and film placement. Neither pattern proves a cause. Ask the equipment supplier to assess the mechanical contact; do not add shims or compensate by increasing pressure from a photograph.

Note whether the film is already wrinkled before pressing or only appears wrinkled afterwards. Edelstein treats these as separate investigation paths: the first directs attention toward feeding and presentation, while the second also calls for review of the pressing conditions and film behaviour. A wrinkle is an observation to locate, not automatic proof that a PET cup is defective.

Check the record of filling as well as sealing. Product on the intended contact area can interrupt bonding, as Edelstein’s contamination guidance explains. Photograph visible splashes or residue before closure when this is safely possible. Increasing temperature does not establish that the contaminated area has been corrected. The practical question is whether the filling process delivers a suitable sealing surface.

Build a timeline before comparing changes

Write a short timeline: what was last recorded as acceptable, what changed, and when the first fault was noticed. Relevant changes can include a cup batch, film roll, print job, tooling change, cleaning intervention or saved recipe. A fault appearing after a change is a lead to investigate, not proof that the changed component caused it. If no acceptable run was documented, say so; do not label an earlier run as a successful reference.

Where the suppliers approve a comparison, keep the other documented conditions fixed and record one identified change at a time. Do not reintroduce damaged components or exceed the equipment or material limits to recreate a failure. Decide the test method and acceptance criteria before the comparison; this article supplies no universal sample count or passing leak rate.

For example, a hypothetical shop starts seeing off-centre film after changing rolls. Its earlier notes contain no film-position photographs. The sensible next step is to document the new roll’s identity and position, then have the equipment and film suppliers check the roll format and approved setup. Ordering a new cup batch or increasing heat at the same time would make the next result harder to interpret. This is an illustrative decision, not a WJPETCUP test or customer case.

Keep bonding, roll sticking and opening behaviour separate

For a weak bond, record the film grade, sealing side and settings. Cattie Adhesives distinguishes platen temperature from the sealing interface; a display alone cannot establish bonding conditions. Confirm the operating range with the suppliers.

For difficult unwinding, record the roll batch and where the symptom starts. Cattie describes layer-to-layer sticking in coated rolls, but that does not diagnose your roll.

For an opening complaint, record where separation or tearing occurs and whether chilling changes the result. Compare with the agreed opening and containment checks; easy peeling is not itself evidence of leakage.

Send a decision-ready record, then verify the changed combination

Give the cup, film and equipment suppliers the same short record, so each is responding to the same event. State what remains unknown. An equipment technician’s proposed repair is not a cup-material approval, and a film supplier’s grade recommendation is not evidence that the finished pack passed.

After an approved intervention, repeat the relevant agreed checks under the intended filling, holding, handling and opening conditions. Keep the resulting decision attached to the exact components and setup. A single pack looking better is useful feedback but does not replace the agreed acceptance assessment. Record any unresolved observation rather than declaring the whole system approved.

Record any cleaning performed during the investigation, including when it produces no improvement. Follow the exact equipment manual for the permitted method and inspection interval, and record what was found and when the work was performed. A cleaning frequency published for another machine is not a maintenance schedule for yours. The sample-approval record guide can hold the final evidence once the problem has been investigated.

Make the handoff answerable by the right party
PartySendAsk for
Cup supplierExact cup model/version and carton or batch identification; unused and failed sample references; rim photographs.Relevant cup/rim information and review of the identified samples, with any limits or missing evidence stated.
Film supplierRoll manufacturer, grade, batch, thickness and format; winding/sealing-side information; breakage or separation photographs.Confirmation of intended substrate and roll specification, plus the next material checks appropriate to the symptom.
Equipment supplier or authorized technicianMachine and installed tooling references; recorded conditions, error display and safely obtained cycle observations.Model-specific checks and an approved intervention or comparison; no copied settings from another machine.

Read more

Discuss the cup evidence in a sealing investigation

For a WJPETCUP cup enquiry, send the cup model and batch reference, rim photographs and the film and equipment details already known. Identify whether you are choosing a new combination or investigating a problem with an existing one, so the relevant cup information can be reviewed.

Back to sourcing guide